ภาพปกงานวิจัย Use epoxidized natural rubber as coupling agent for reinforcement calcium carbonate filled natural rubber

The reduction of calcium carbonate (CaCO3) particle was prepared by wet grinding method with 40% dispersion. The particle sizes of CaCO3 were studied with various time of wet grinding. It was found that the particle sizes of CaCO3 rapidly decreased in 3 day of grinding after that it was slightly reduce. Therefore the CaCO3 at various time of wet grinding were mixed with concentrate latex (60% dry rubber content DRC). The result showed that the wet grinding for 2 days provided the superior machanical properties. In addition the compound with epoxidized natural rubber (ENR) as a coupling agent was investigated. It was found that the 5 phr of 30% mole percent of ENR results in significantly improved mechanical properties of the rubber vulcanizates.

APA

สายจันทร์, เดี่ยว. รัตนพันธ์, สุวัฒน์. ( 2558 ). Use epoxidized natural rubber as coupling agent for reinforcement calcium carbonate filled natural rubber. กรุงเทพมหานคร.

Chicago

สายจันทร์, เดี่ยว. รัตนพันธ์, สุวัฒน์. Use epoxidized natural rubber as coupling agent for reinforcement calcium carbonate filled natural rubber. กรุงเทพมหานคร: มหาวิทยาลัยเทคโนโลยีราชมงคลพระนคร, 2558.

MLA

สายจันทร์, เดี่ยว. รัตนพันธ์, สุวัฒน์. Use epoxidized natural rubber as coupling agent for reinforcement calcium carbonate filled natural rubber. กรุงเทพมหานคร, 2558.

Vancouver

สายจันทร์, เดี่ยว. รัตนพันธ์, สุวัฒน์. Use epoxidized natural rubber as coupling agent for reinforcement calcium carbonate filled natural rubber. กรุงเทพมหานคร; 2558.