จำนวน Repository ( 17 )

การออกแบบแม่แบบเครื่องจักสานผักตบชวาจากน้ำยางพาราเพื่อลดต้นทุนในการผลิตและพัฒนาผลิตภัณฑ์เครื่องจักสานผักตบชวา
การออกแบบแม่แบบเครื่องจักสานผักตบชวาจากน้ำยางพาราเพื่อลดต้นทุนในการผลิตและพัฒนาผลิตภัณฑ์เครื่องจักสานผักตบชวา

The objectives of this research were 1) to study the design and experiment of materials for producing water hyacinth basketry templates from para rubber 2) to test the water hyacinth basketry templates from para rubber 3) to create a body of knowledge in the development of water hyacinth basketry templates. from rubber latex to the community The process of operation is to design the shape of a water hyacinth basketry to suit the use of the product first after that create a water hyacinth basketry template from para rubber by experimenting with a formula mixed with natural rubber latex and experiment with weaving vegetables. water hyacinths to find the best techniques and styles Results from research on the design of water hyacinth wicker templates from rubber latex and testing of water hyacinth wicker template designs from rubber latex. The aim is to invent materials to solve the problem of replacing the old wicker template. From the research it was found that the water hyacinth basketry model was made from rubber latex. There are two techniques for creating new templates: removable templates and removable templates. and non-removable templates Removable latex coated wicker template can produce many pieces easy to weave The wicker template part is coated with rubber latex. Non-removable or weave cover It can be used to weave as a furniture product with the properties that were discovered that it has a long service life. It is durable strong and durable. Flexibility to reduce shock during weaving. and can be a tool in the profession Can reduce the cost of producing water hyacinth handicrafts Model development part There is a design template for water hyacinth basketry which is a water hyacinth wicker product that has a shape that is exotic modern beautiful and useful according to the products unique characteristics and is a valuable work that can decorate the house beautifully.

2566
การผลิตวัสดุปรับปรุงดินจากเศษอาหารและผักตบชวาด้วยกรรมวิธีดีไฮเดรชั่น
การผลิตวัสดุปรับปรุงดินจากเศษอาหารและผักตบชวาด้วยกรรมวิธีดีไฮเดรชั่น

The purpose of this study is to produce the soil improvement materials from food waste and water hyacinth by using a dehydration process. The experiments were divided into two parts : 1) the study of the optimum temperature and time for converting food waste and water hyacinths to soil improvement materials by determining the temperatures of 100 °C 150 °C and 200°C in the periods of 1 hour 2 hours and 3 hours respectively 2) the study of nutrient content in the materials before and after mixing into the soil for 5 days. The soil used in the experiment was sampled from Sai Ma Subdistrict Nonthaburi Province. The parameters used to evaluate the ability to improve the soil quality were soil moisture pH electro conductivity total nitrogen total phosphorus total potassium and organic matter. The results showed that the optimum temperature for drying the food waste was 150°C for 2 hours and the optimum temperature for drying the water hyacinth was 200°C for 3 hours. When the materials were mixed into soil it found that the soil drainage was improved. Mixing the materials into soil could increase the pH value from 5.2 to 5.4 and increase the electrical conductivity from 0.72 mS/cm to 14.78 mS/cm. Besides the plant nutrients including Nitrogen phosphorus and potassium also increased after adding soil improvement materials.

2565
การควบคุมคุณภาพการย้อมสีและตกแต่งสำเร็จเส้นด้ายผักตบชวาและวัสดุประกอบเพื่อการแปรรูปผลิตภัณฑ์เชิงพาณิชย์
การควบคุมคุณภาพการย้อมสีและตกแต่งสำเร็จเส้นด้ายผักตบชวาและวัสดุประกอบเพื่อการแปรรูปผลิตภัณฑ์เชิงพาณิชย์

Quality control of dyeing and finishing of Water Hyacinth yarns and their transformed materials for commercial was a main objective to establish the dye database of synthetic dye and natural dye. The dye database was a data for quality control in dyeing process of raw material as Water Hyacinth yarns also it resolved the un-repeatability dyeing problem. Reactive dye was used for synthetic dye database creation on dry Water Hyacinth yarns at 80oC for 30 minutes. Red as Hicion Red He-3B yellow as Hicion Yellow HE-4RN Blue as Hicion Navy Blue HER 150% and black as Hifix Black KNN were the represent synthetic dye and Sodim sulphate 20 g/l and sodium carbo nate 20 g/l were used as auxiliaries. The other hands the natural dye database was forming from Ebony tree Caesalpinia sappan and Turmeric. They were dye on dry Water Hyacinth yarns at 80oC for 30 minutes and Sodim sulphate 20 g/l was the auxiliary. Whereas Butterfly pea were dye at 80oC for 30 minutes by Sodim sulphate 20 g/l and sodium carbonate 20 g/l were the auxiliaries. The whole dye database was defined the totally in Primary Secondary and ternary dye cycle. The transfer knowledge was distributed to the enterprise at Nakhon Prathom Provincd as “Chumchonjaksanpaktobchawha Bann klongnokkratum”. The topics were “How to establish the synthetic and natural dye database” “Water repel lent finishing” and “developed and transformed the Water Hyacinth to products”. The target group was very satisfied in this topic as 4.39. In the result the proportion between economic and social factor by the income increasing in 1 year was 5.04. So the research project was achievement.

2563
การใช้ประโยชน์จากเส้นใยผักตบชวาในผลิตภัณฑ์แผ่นใยอัดซีเมนต์ภายนอกอาคารสำหรับวิสาหกิจชุมชน
การใช้ประโยชน์จากเส้นใยผักตบชวาในผลิตภัณฑ์แผ่นใยอัดซีเมนต์ภายนอกอาคารสำหรับวิสาหกิจชุมชน

This research aims to study the water hyacinth fiber inside high-density fiber cement board. By using ratio components among cement : fine sand : water hyacinth fiber : water : catalyst accelerated the formations of cement (aluminum sulfate (AI2 (SO4) 3) calcium chloride (CaCl2) sodium silicate (Na2SiO3)) on the ratio 1: 0.2: 0.075: 0.3: 0.03 by weight of total water hyacinth fiber with the steel grating inside. By compressing the mixture cast machine at normal temperature (30 - 35 °C). From the test results the ratio of B4 is the appropriate ratio from the 1st year research result to produce the high-density fiber cement board with the steel grating inside 0.81mm #0.5”. It can pass the TIS 878-2537 standard of Cement Board and good based-on high density and physical properties mechanical properties and thermal insulation. Accelerate the formation of the most suitable cement is calcium chloride (CaCl2).

2563
การศึกษาส่วนผสมที่เหมาะสมของโครงสร้างกันแรงกระแทกของรถยนต์จากกากผักตบชวาและแกลบสำหรับการชนคนเดินเท้า
การศึกษาส่วนผสมที่เหมาะสมของโครงสร้างกันแรงกระแทกของรถยนต์จากกากผักตบชวาและแกลบสำหรับการชนคนเดินเท้า

Recently the Thai industry has continually grown up and also plays a role to economic growth in the country which affects the many of automotive components to be in the market. While the degeneration and waste of automotive components had increased as well. Therefore a crash box is one of the automotive parts which damage from the accident. Consequently the researchers have created a prototype material to develop into the crash box to reduce the environment problem from automotive parts. The random mixture of water hyacinth and husk was attempted to up to 5 ingredients. By forming a solid cylinder and 200 mm of long was used as prototype of the crash box in this research. Thus the energy absorption using compressing test was attempted to by the universal testing machine. The results showed that using polymers as a binder with 50% of water hyacinth and 50% of husk was the better ability of energy absorption. Regarding this ingredient 1612444 J/m3 of the energy absorption was referred to indicate that is the best ability of energy absorption. It is probably reduce the severity of the impact in the event of pedestrian collision.

2563