จำนวน Repository ( 9 )
การใช้ประโยชน์เศษหินบะซอลต์เนื้อโพรงข่ายเป็นมวลรวมในแผ่นซีเมนต์บอร์ดสำหรับผนังอาคารถอดประกอบ
This research aims to develop the cement board from vesicular basalt fragment. The 5 ratios of Portland cement type1: fine sand: vesicular basalt fragment: sodium silicate: tap water are equal to 1: 2: 0: 0.03: 0.5 1: 2: 2: 0.03: 0.5 1: 2: 4: 0.03: 0.55 1: 2: 6: 0.03: 0.6 and 1 : 2 : 8: 0.03: 0.65 by weight. The cement boards were produced by compression machine. The property tests of cement-bonded fiberboard followed the TIS. 878-1994 standard (cement bonded particle board: high density). From the results 1: 2: 4: 0.03: 0.55 is the most suitable ratio of cement board from coconut shell ash. This developed cement boards can apply the vesicular basalt fragment to use as the construction materials with light-weight high strength good thermal insulation and moisture protection properties
อาคารสำเร็จรูปครึ่งทรงกลมจากโครงสร้างเหล็กแบบถอดประกอบง่าย
The objectives of this research are to develop the structure to create the knowledge of construction technology to test the properties to construction the prototype building and to transfer the technology of hemisphere pre-engineered building with easy assembly steel structure type. The load and resistance factor design (LRFD) method was used to design the structure by regarding the strength material type construction and deconstruction step and cost. From the design the prototype of hemisphere pre-engineered building (only the frame structure) was construction with 5 meters of diameter 3.5 meters of height 19.635 square meters of useful space 200000 Baht of material cost (10186 Baht per square meter for all materials) 27 hours or 3 days of construction period. According to the modular coordination system this hemisphere pre-engineered building cans construction and deconstruction fast especially when apply to help disaster victims. After tested the structure that the calculation value of safety factor (S.F.) is 1.76. The envelope of this building used the ratio of Portland cement type 1: fine sand: coconut fiber: waterproofed liquid: tap water which equal to 1:3: 0.1: 0.02: 0.5 by weight and reinforced by round bar and wire mesh steel. According to the testing the building-envelope properties are following: density 1582 kg/m3 thermal conductivity coefficient 0 .3 7 1 watt/m.Kelvin water absorption 1 7 .3 1 % compressive strength 118.47 ksc and bending strength 28.88 ksc. Moreover these results can register the copyright and draft the research paper to transfer the technology for target group.
การใช้เศษโฟมเหลือทิ้งจากบรรจุภัณฑ์สำหรับผลิตเป็นแผ่นผนังคอนกรีตสำเร็จรูปน้ำหนักเบา
The objectives of this research are to study the production to find the proper ratio to test the physical mechanical properties and thermal conductivity to suggest the implementation and to transfer the technology of light-weight precast concrete wall panel products mixed with container foam wastes. Design the ratios of Portland cement type1: coarse sand: lime stone: water equal to 1: 2: 4: 0.7 by weight and adding the container foam wastes equal to 0 0.025 0.050 0.075 and 0.1 by weight. Casting the light-weight precast concrete wall panel products by pouring the concrete into the mold which installed the steels. Test the properties follow TIS.2226-2548 and TIS.878-2537. From the results the proper ratio of adding container foam wastes was 0.075 by weight which had perfect general characteristic 16.48 MPa of compressive strength no bending when installed in common behavior 8.86% of water absorption passed type1 of hardness test passed type 2 of impact test 2014.54 kg/m3 of density 4.30 MPa of bending strength and 0.228 watt/m.K of thermal insulation. This light-weight precast concrete wall panel product can use as the thermal insulation wall in building. Moreover the developing product can apply to register the petty patent.
การใช้เถ้ากะลามะพร้าวเป็นมวลรวมน้าหนักเบาในคอนกรีตบล็อกเพื่อการประหยัดพลังงาน
The objectives of this research are to study the production step proper ratio physical properties mechanical properties thermal insulation and sound insulation efficiency of concrete blocks mixed with coconut shell ash. The ratios of concrete block mixed with coconut shell ash include Portland cement type1: quarry dust: coconut shellash which equal to 1: 6.8: 0.2 1: 6.7: 0.3 1: 6.6: 0.4 1: 6.5: 0.5 and 1: 6.4: 0.6 by weight. Water per cement ratio are 0.6 by weight. The concrete block samples were casted by the general production as same as the ordinary concrete blocks and were tested follow TIS.58. From the results the best amount of coconut shell ash which put into concrete block is 1: 6.7: 0.3 of ratio. The proper ratios of coconut shell ash can decrease the density or weight and increase the thermal insulation and sound insulation efficiency of concrete blocks. However the high amounts of coconut shell ash effect to decrease the mechanical properties concrete blocks that are lower than TIS.58 standard.