จำนวน Repository ( 29 )

การใช้เทคโนโลยีสำหรับชุมชนการพัฒนาผลิตภัณฑ์บล็อกประสานจากเศษหินบะซอลต์
การใช้เทคโนโลยีสำหรับชุมชนการพัฒนาผลิตภัณฑ์บล็อกประสานจากเศษหินบะซอลต์

This research aims to study the using basalt rock fragments to develop as interlocking block product. The mixture ratios of Portland cement type1: basalt rock fragments are 11 : 6 1 : 6.5 1 : 7 1 : 7.5 and 1 : 8 by weight and water per cement ratio was 0.6 by weight. The interlocking block samples are cast in 10 x 20 x 10 cubic centimeter of dimension with manual compression molding machine. The interlocking block samples were tested in accordance with TCPS 602-2547 standard which subjected for the interlocking block. The results show that the weight compressive strength and thermal conductivity of interlocking blocks with high quantity of basalt rock fragments are lower than interlocking blocks with low quantity of basalt rock fragments while that the water absorption of interlocking blocks with high quantity of basalt rock fragments are higher. From this research the medium and small enterprises could choose the proper ration for the interlocking block production mixing basalt rock fragments as per requirement.

2561
การออกแบบชุดทำงานสตรีด้วยเทคนิคการตีเกล็ด จากผ้าทอบ้านเขาเต่า อำเภอหัวหิน จังหวัดประจวบคีรีขันธ์
การออกแบบชุดทำงานสตรีด้วยเทคนิคการตีเกล็ด จากผ้าทอบ้านเขาเต่า อำเภอหัวหิน จังหวัดประจวบคีรีขันธ์

The objectives of this study were 1) to explore the using tucks technique and Ban Khao Tao Woven Fabric Hua Hin Prachuap Khiri Khan. 2) to design of Women’s Working Dress by Tucks Techique from Ban Khao Tao Woven Fabric Hua Hin Prachuap Khiri Khan. 3) to explore the Women’s Working Dress satisfactions to wards the design of Women’s Working Dress by Tucks Techique from Ban Khao Tao Woven Fabric Hua Hin Prachuap Khiri Khan. The sample of this was 385 working women from the government commemorating His Majesty the King’s 80th Birthday Anniversary 5th December B.E. 2550 (2007). The research instrument was the questionnaire and 12 prototype sets of Women’s Working Dress by Tucks Techique consisting of coatsskirts and dresses. In this study. From the study it is found that most of the respondents are of above 35-45 years old married master-degree-graduated office women with average income of more than 35001 baht. Most of them had ever bought/worn fabric clothing with woven fabrics in Khaotao. The reason for buying such cloths is “buy when they would like to”. The frequency of buying the cloth is “3 month”. Furthermore the prices of their working cloths are around 1500-2000 baht each. From the study of respondents’ satisfaction on the Women’s Working Dress it is found that the most satisfactory dress second kind more than the first of 4.08 and the third kind with the average score of 4.07 4.05and 4.02 respectively. The most satisfactory coat is the coat of the third kind second and the first 4.14 kind with the average score of 4.134.12 and4.02 respectively. For the skirts the most satisfactory one is of the first 4.13 kind third and the second kind with the average score of4.074.05and4.05 respectively.

2561
การพัฒนาขนมหินฝนทองด้วยแป้งข้าวไรซ์เบอรี่ทดแทนแป้งข้าวเจ้าบางส่วน
การพัฒนาขนมหินฝนทองด้วยแป้งข้าวไรซ์เบอรี่ทดแทนแป้งข้าวเจ้าบางส่วน

This research study the purposes of the research are to : 1) to study the standard formula Hin Fon Thong dessert. 2) to study the recipe of Hin Fon Thong dessert. Developed with Partially substituted riceberry rice flour for rice flour has been accepted and 3) to study nutrition and nutritional value between the standard formula Hin Fon Thong dessert. With development of Hin Fon Thong dessert partially substituted riceberry rice flour has been accepted. This study aimed to develop a more nutritious dessert to answer modern needs and to conserve custom through old Thai dessert. Experts in various related aspects were interviewing. Method of preparation was adapt using scientific principle to produce a dessert as close to the original recipe as possible. It was further developing through the use of riceberry rice flour in place of rice flour which was the main ingredient of the dessert. Acceptability was test when varying ratio between riceberry rice flour and rice flour were used. Four levels of rice flour and riceberry rice flour were 75:25 80:20 85:15 and 90:10. Sensory test used the 9 - point hedonic method The results showed that : The top score is the 85:15 with the lowest score was at 8.03 and the highest score was at 8.33. The analysis continues to test on the general public with other components: taste product design and willingness to buy the product. By using percentage statistics. Average score was over 50:100. The survey shows that most people moderately like the dessert. It was recommended that it should slightly reduce the sweetness should be slightly reduced. By comparing the original rice flour Hin Fon Thong and the new 85:15 ratio of riceberry rice flour Hin Fon Thong the difference is the in oreased amount of highly nutritious substances like vitamin E beta carotene omega - 3 folate polyphenols tannins gamma - original. and antioxidants gained from the new riceberry rice flour recipe. Calculated from the INMUCAL Nutrients program Therefore one unit that is suitable for the riceberry rice Flour Hin Fon Thong is 5 - gram or equivalent to 1 piece.

2561
การใช้เทคโนโลยีสำหรับชุมชนในการพัฒนาผลิตภัณฑ์บล็อกปูพื้นลดอุณหภูมิจากเศษหินพัมมิช
การใช้เทคโนโลยีสำหรับชุมชนในการพัฒนาผลิตภัณฑ์บล็อกปูพื้นลดอุณหภูมิจากเศษหินพัมมิช

This research aims to study the usage pumice rock fragments to develop paving block product for community. The mixture ratios of Portland cement type1: sand: quarry dust: pumice rock fragments: water that there are 6 ratios. The paving block samples are casted in 30 x 30 x 5 centimeter in dimension. The paving block sample testing follows the TIS 378-2531 on concrete flooring tiles. From the experiment bending strength and thermal conductivity of paving blocks with high quantity of pumice rock fragments are lower than paving blocks with low quantity of pumice rock fragments but the water absorption of paving blocks with high quantity of pumice rock fragments are higher. However all of pumice rock fragments paving block samples with lower than 1: 2: 2.4: 0.6: 0.6 of ratio can pass the standard and the surface temperature is lower than other covering materials about 2 degree Celsius.

2560
การใช้เทคโนโลยีสำหรับชุมชนในการพัฒนาผลิตภัณฑ์บล็อกประสานลดอุณหภูมิจากเศษหินพัมมิซ
การใช้เทคโนโลยีสำหรับชุมชนในการพัฒนาผลิตภัณฑ์บล็อกประสานลดอุณหภูมิจากเศษหินพัมมิซ

This research aims to study how to use stones Pumice Products is interlocking block for community development. The mixture ratios of Portland cement type1: sand: quarry dust: pumice rock fragments: water that there are 5 ratios. The products were tested by the community TCPS 602-2547 (2004) (Thai): interlocking block. The results showed that interlocking block of stone pumice much a compressive strength and thermal conductivity under a block of stone pumice less. The water absorption is increased When a block of stone pumice much. The optimum ratio and the use of waste rock Pumice highest ratio of cement to stone dust on the stone Pumice water in a 10: 6.4: 0.6: 0.45 to 10: 6.1: 0.9. 0.45 by weight.