การใช้เทคโนโลยีสำหรับชุมชนในการพัฒนาผลิตภัณฑ์ คอนกรีตบล็อก ลดอุณหภูมิจากเศษหินพัมมิซ
This research aims to produce scrap page kaolin of brick construction. The kaolin clay ratio of 100: 0 80:20 60:40 50:50 40:60 20:80 and 0: 100 by volume Add mixed with rice husk and rice 15 percent by weight A total of seven ratios. According to standard tests or TIS. 77-2545 ordinary story brick building. The moisture content and water absorption is increasing. While density Thermal conductivity resistance flexural and compressive strength tends to decrease. The best ratio of 80:20 by volume with compressive strength 43.16 kg / cm 2 and 24.93 percent water absorption. Criteria standard of TIS. 77-2545 requiring compressive strength not less than 35 kg / cm2 and water absorption must not be higher than 25 percent. Can be used in the manufacture of brick construction including building decorative wall can be developed into products. Because skin color and beautiful
การพัฒนาวัสดุอาหารจากวัสดุเหลือทิ้งทางการเกษตรเพื่อการประหยัดพลังงานและลดการถ่ายเทความร้อนเข้าสู่อาคาร
The objective of this research is to study the implementing the agricultural residue to the design of outdoor paving block for lowering the building temperature. The base layer admixture (layer no.1) is selected from cement type1: quarry dust: rice husk: rice straw: water ratios equal to 1: 3: 0: 0: 0.3 1: 1: 0: 1: 0.5 1: 1. 0.25: 0.75: 0.5 1: 1: 0.5: 0.5: 0.5 1: 1: 0.75: 0.25: 0.5 and 1: 1: 1: 0: 0.5 by weight. The surface layer admixture (layer no.2) is white silica cement: yellow stone chip no.4: water equals to 1: 4: 0.3 by weight. The exterior floor-covering blocks were tested following density testing water absorption testing compressive testing and surface temperature testing compare with laterite sandstone paving concrete block marble and granite. Resulting the best ratio of cement type1: quarry dust: rice husk: rice straw: water is 1: 1: 0.75: 0.25: 0.5 that has properties at 28 days following 1939.43 kg/m of density 14.97 % of water absorption 284.69 ksc of compressive strength and lower than other paving blocks around 3 – 13 degrees Celsius of surface temperature